LATEST UPDATESEnglish
AABGOA NewsA curated stream of attributed news links
Stay close to the storiesA clear view of source-attributed news headlines.
Technology

Fermented Beverage Yeasts Enable Eco-Friendly Zinc Oxide Coatings That

Materials scientists and bioprocess engineers have successfully demonstrated an environmentally benign route for fabricating antimicrobial surface coatings by using unconventional yeast strains recovered from traditional fermented beverages to synthesize zinc

Illustrative imageIllustrative image

Materials scientists and bioprocess engineers have successfully demonstrated an environmentally benign route for fabricating antimicrobial surface coatings by using unconventional yeast strains recovered from traditional fermented beverages to synthesize zinc oxide nanostructures. The investigation, documented by researchers Gülden Kılıç, Gökhan Gurur Gökmen, and Yogendra Kumar Mishra, harnessed cell-free extracellular extracts from wild-type yeasts present in artisanal kombucha and beetroot kvass to drive the biological reduction and nucleation of zinc oxide nanoparticles. Unlike conventional chemical and physical fabrication protocols that frequently rely on toxic reagents, aggressive reducing chemicals, and energy-intensive manufacturing environments, this biological approach harnesses metabolic secretions to generate functional nanomaterials under mild ambient conditions. Beyond synthesizing colloidal nanoparticles, the researchers deposited the biogenic materials onto glass substrates using a multi-step spin-coating procedure followed by controlled thermal annealing at 400 degrees Celsius to yield coherent nanoscale coatings. Comprehensive biological evaluations revealed that while the resulting thin films exhibited limited diffusive clearance zones in conventional agar assays, direct physical contact between the coated substrates and pathogenic bacterial suspensions achieved complete microbial inactivation within two hours, establishing a sustainable nanotechnology platform for prospective applications across active food packaging, hygiene maintenance, and biomedical device protection.

The study addressed a critical challenge in modern nanomaterials engineering by exploring sustainable synthesis methods that overcome the economic and environmental penalties associated with standard top-down physical milling and bottom-up chemical precipitation. To source the required biological platforms, the research team collected spontaneously fermented beverages from a local producer in Alanya, Antalya, Türkiye, including artisanal ginger kombucha, black mulberry kombucha, and red beetroot kvass. Microbial enumeration of the pristine fermented liquid samples revealed viable yeast populations spanning from 3.74 to 5.07 log colony-forming units per milliliter. Following selective plating, purification on malt extract agar, and morphological evaluation, nine distinct yeast isolates were recovered from the beverage matrices. Three representative strains, designated M1 from ginger kombucha, M2 from black mulberry kombucha, and M3 from red beetroot kvass, were selected for full taxonomic and functional exploration. Sanger sequencing of the internal transcribed spacer rDNA region, encompassing the ITS1, 5.8S, and ITS4 domains, identified isolate M1 as Zygosaccharomyces bailii, deposited under GenBank accession PV200289, and isolates M2 and M3 as Brettanomyces anomalus, cataloged under accessions PV200294 and PV219289, respectively, marking the inaugural application of these specific non-conventional yeasts as bio-factories for metallic nanomaterials.

Selected yeast isolates were cultured in potato dextrose broth at 25 degrees Celsius for 48 to 72 hours and subsequently centrifuged at 10,000 revolutions per minute to remove cellular biomass, ensuring that downstream processing remained free from complex cell-lysis steps. For each experimental reaction, 100 milliliters of the resulting cell-free supernatant adjusted to pH 7.5 was combined with 50 milliliters of 0.1 molar aqueous zinc acetate solution. These mixtures were incubated under continuous mechanical agitation at 150 revolutions per minute and maintained at 37 degrees Celsius for 24 hours. The progress of the biological reduction was visually evidenced by a clear color transition from an initial translucent light brown to a dense pale or milky white suspension. The resulting particulate biomass was harvested by repeated centrifugation at 10,000 revolutions per minute, thoroughly washed four consecutive times with distilled water to purge residual nutrient broth constituents, and dried in a drying oven at 40 degrees Celsius for 18 to 24 hours to produce dry zinc oxide nanopowders designated ZnO-1, ZnO-2, and ZnO-3.

Transitioning the synthesised nanopowders into functional, surface-bound antimicrobial barriers required a reproducible and controlled deposition strategy. The research team employed spin coating to convert the biogenic powders into uniform thin films supported on pre-cleaned glass slides measuring two by two centimeters. Substrates were sequentially subjected to fifteen-minute ultrasonic cleaning cycles in high-purity acetone, isopropanol, and distilled water to ensure pristine surface bonding conditions. The synthesized zinc oxide nanoparticles were homogeneously dispersed in seventy percent aqueous ethanol at a concentration of one percent weight by volume to formulate the liquid deposition suspensions. Aliquots of these dispersions were dropped onto the spinning glass substrates at a rotational velocity of 3,000 revolutions per minute for sixty seconds under controlled ambient conditions. Each deposited wet layer was immediately dried on a hot plate at 90 degrees Celsius for ten minutes to evaporate the carrier solvent, a cyclic coating sequence that was executed three times per specimen to establish uniform coverage. Finally, the layered substrates underwent furnace annealing at 400 degrees Celsius for one hour to densify the deposited particulate matrix and enhance mechanical adherence between the film and underlying glass.

Detailed spectroscopic and microscopic analyses verified the successful synthesis of the nanostructures and exposed dramatic structural differences among the derived thin films. Ultraviolet-visible absorption spectroscopy demonstrated characteristic absorption bands centered near 300 nanometers for both the colloidal nanoparticle suspensions and their respective thin films, confirming electronic transition profiles intrinsic to nanoscale zinc oxide. Transmittance measurements across visible wavelengths between 400 and 700 nanometers indicated that thin films fabricated from isolate M3 exhibited noticeably greater optical clarity than those prepared from M1 or M2. Scanning electron microscopy revealed that the biosynthesized nanoparticles predominantly assumed aggregated clusters of hexagonal and quasi-spherical geometries, a phenomenon influenced by interparticle electrostatic attractions and capping biomolecules. Cross-sectional electron micrographs demonstrated that despite identical deposition parameters, film thickness varied widely depending on the biological origin: ZnO-1 formed thin layers of 516.09 plus or minus 67.60 nanometers, ZnO-2 produced an exceptionally thick coating measuring 34.37 plus or minus 4.81 micrometers, and ZnO-3 measured 1.48 plus or minus 0.08 micrometers, highlighting that microbial metabolites fundamentally govern film assembly and packing behavior.

Elemental composition and spatial distribution were systematically evaluated through energy-dispersive X-ray spectroscopy to confirm the purity and chemical uniformity of the materials. The spectra obtained from the nanoparticle powders presented a prominent characteristic electronic emission peak near 1 kiloelectronvolt corresponding to zinc alongside a medium-intensity signal corresponding to elemental oxygen, with no extraneous inorganic contamination detected. Quantitative elemental analysis revealed atomic percentages of 12.89 percent zinc and 33.29 percent oxygen for ZnO-1 nanoparticles, 11.79 percent zinc and 36.13 percent oxygen for ZnO-2 nanoparticles, and 11.76 percent zinc and 44.35 percent oxygen for ZnO-3 nanoparticles. Analysis of the annealed thin films demonstrated zinc contents of 8.30 percent, 7.55 percent, and 6.60 percent alongside corresponding oxygen proportions exceeding ninety percent, reflecting signal contributions from the underlying silicate substrate and surface hydroxylation. Minor trace signals of carbon, nitrogen, and phosphorus detected across spectra were associated with residual biological metabolites originating from the yeast culture media. Elemental mapping corroborated that both zinc and oxygen atoms were evenly dispersed across the film surfaces without localized segregation, confirming consistent spatial homogeneity across all coated substrates.

Crystallographic examination using X-ray diffraction exposed fundamental differences between the free nanopowders and the thermal-annealed thin films. Powder diffraction patterns for the green-synthesized particles exhibited well-defined peaks corresponding to the (111) and (041) crystallographic reflection planes, confirming good crystallinity and indicating the coexistence of cubic structures alongside monoclinic Zn20O48 crystalline phases. Applying the Scherrer equation to the dominant diffraction peaks yielded nanoscale crystallite dimensions of 10.80 nanometers for both ZnO-1 and ZnO-2, while ZnO-3 nanoparticles synthesized by Brettanomyces anomalus M3 exhibited crystallite sizes of 8.78 nanometers at two-theta equal to 33.47 degrees and 19.40 nanometers at two-theta equal to 59.74 degrees. In sharp contrast, the spin-coated and annealed thin films displayed no discernible diffraction reflections, revealing an essentially amorphous or weakly ordered structural state. The authors noted that annealing at 400 degrees Celsius was insufficient to overcome the structural disruption caused by residual organic capping species adsorbed on the nanoparticle boundaries, which suppressed long-range crystal growth and atomic lattice alignment during thermal consolidation.

Fourier transform infrared spectroscopy and static water contact angle measurements uncovered the interfacial surface chemistry and wettability characteristics driving material functionality. Infrared spectra identified absorption bands between 519 and 631 inverse centimeters assigned to fundamental zinc-oxygen stretching vibrations, verifying core oxide lattice formation. Broad absorption peaks between 3,319 and 3,350 inverse centimeters revealed abundant surface hydroxyl groups, while bands at 2,959 to 2,961 and 2,887 to 2,893 inverse centimeters corresponded to alkane carbon-hydrogen stretching, and bands near 1,390 and 1,560 inverse centimeters reflected carbonyl and alkene groups associated with yeast-secreted proteins and flavonoids. Goniometric surface analysis demonstrated that all fabricated coatings maintained a hydrophilic profile with water contact angles strictly below 40 degrees. Uncoated glass presented an angle of 28.24 degrees, which shifted to 33.87 degrees for ZnO-1, 25.07 degrees for ZnO-2, and 33.17 degrees for ZnO-3. Although ZnO-2 exhibited the lowest contact angle and greatest surface hydrophilicity, these wetting characteristics did not directly correlate with biological efficacy, indicating that surface energy alone does not govern bacterial neutralization.

Evaluation of antibacterial activity in liquid suspensions and agar diffusion assays demonstrated potent antimicrobial potency against foodborne model pathogens. Testing against Gram-negative Escherichia coli O157:H7 and Gram-positive Staphylococcus aureus ATCC 6538P via the agar-well diffusion method showed that colloidal nanoparticle suspensions generated wide zones of growth suppression ranging from 13.00 plus or minus 2.12 to 22.00 plus or minus 0.71 millimeters, with Zygosaccharomyces bailii-derived ZnO-1 displaying the highest potency. Broth microdilution confirmed minimum inhibitory concentrations between 0.313 and 0.625 milligrams per milliliter and minimum bactericidal concentrations ranging from 0.313 to 1.25 milligrams per milliliter for both organisms. However, when the thin-film-coated glass substrates were evaluated using the modified Kirby-Bauer disk diffusion method, they generated modest or undetectable clearance rings: ZnO-3 produced a zone of only 1.25 millimeters against Escherichia coli and 0.00 millimeters against Staphylococcus aureus, while ZnO-2 yielded 0.50 and 1.00 millimeter zones, and ZnO-1 showed no inhibition against Staphylococcus aureus, reflecting the physical entrapment and poor diffusive mobility of solid zinc oxide through agar media.

The definitive functional capability of the biosynthesized thin films was revealed through direct-contact testing, which mirrored real-world surface exposure. When bacterial suspensions carrying approximately 10,000 colony-forming units per square centimeter of Escherichia coli O157:H7 and Staphylococcus aureus were inoculated directly onto the coated surfaces, viable cell enumeration showed that all developed thin films achieved complete, one-hundred-percent bacterial eradication within two hours of room-temperature exposure. Drawing upon characterization data and microbiological literature, the authors attributed this biocidal mechanism to a synergistic combination of direct membrane envelope disruption, controlled zinc ion release, and surface-catalyzed reactive oxygen species generation, while acknowledging that direct biochemical quantification of free radicals was beyond the empirical scope of the study. The researchers emphasized that optimizing synthesis conditions to regulate particle morphology, crystallite dimensions, and film thickness will be vital for future applications. Nevertheless, the successful integration of food-derived probiotic yeast supernatants into durable, highly active surface coatings establishes a compelling sustainable framework for developing non-toxic antimicrobial barriers in food safety and healthcare.

Subject of Research: Biosynthesis of zinc oxide nanostructures from fermented beverage yeasts and their antibacterial thin film performance

Article Title: Eco-friendly synthesis of ZnO nanostructures from yeast strains isolated from kombucha and beetroot kwass for antimicrobial thin film applications

Article References: Kılıç, G., Gökmen, G. G., & Mishra, Y. K. (2026). Eco-friendly synthesis of ZnO nanostructures from yeast strains isolated from kombucha and beetroot kwass for antimicrobial thin film applications. Bioprocess and Biosystems Engineering, 49(7), 1885-1907. https://doi.org/10.1007/s00449-026-03372-0

Image Credits: AI Generated

DOI: 10.1007/s00449-026-03372-0

Keywords: zinc oxide nanoparticles, green synthesis, thin films, antimicrobial coatings, kombucha, beetroot kvass, Zygosaccharomyces bailii, Brettanomyces anomalus, spin coating, antibacterial activity, Escherichia coli, Staphylococcus aureus, water contact angle, nanotechnology, X-ray diffraction, bioprocess engineering, food safety

News Source: Denise Maddox. (November 26, 2026). Fermented Beverage Yeasts Enable Eco-Friendly Zinc Oxide Coatings That Neutralize Bacteria. Scienmag.