Dispersed Nickel Nanoparticles on Carbon Nanotubes Triple Guaiacol

Chemical engineering researchers have demonstrated that controlling the metallic dispersion of nickel nanoparticles supported on multiwall carbon nanotubes significantly alters catalytic turnover frequency and reaction pathways during the hydrodeoxygenation of

Illustrative imageIllustrative image

Chemical engineering researchers have demonstrated that controlling the metallic dispersion of nickel nanoparticles supported on multiwall carbon nanotubes significantly alters catalytic turnover frequency and reaction pathways during the hydrodeoxygenation of guaiacol, a representative model molecule for raw bio-oil. In continuous gas-phase fixed-bed reactor assessments, a catalyst formulated with two weight percent nickel achieved an intrinsic turnover frequency nearly twice as high as an eleven weight percent nickel formulation and approximately three times higher than a twenty weight percent nickel catalyst. The experimental results reveal that the hydrodeoxygenation of guaiacol exhibits pronounced structure sensitivity over supported nickel, establishing that smaller metallic crystallites possessing high proportions of edge and corner sites accelerate molecular conversion far more effectively than larger agglomerated metallic ensembles across identical operational temperatures.

Conventional catalytic hydroprocessing strategies have historically relied on sulfided cobalt-molybdenum or nickel-molybdenum mixtures supported on gamma-alumina; however, these commercial sulfur-dependent catalysts suffer from rapid poisoning, accelerated phase deactivation, moderate conversion efficiencies, and undesirable residual sulfur contamination within the final hydrocarbon streams.

To overcome these historical limitations, the research team synthesized non-sulfided catalysts utilizing multiwall carbon nanotubes as inert, thermally stable catalytic supports featuring minimal inherent surface acidity. Commercial multiwall carbon nanotubes measuring one hundred ten to one hundred seventy nanometers in outer diameter and five to nine micrometers in length were initially subjected to a thermal cleaning pretreatment within a quartz tube reactor at three hundred degrees Celsius under a continuous hundred milliliter per minute nitrogen sweep for four hours to eliminate residual surface contaminants. The dried carbon nanotubes were subsequently impregnated to their incipient wetness point using aqueous nickel acetate tetrahydrate solutions calibrated to yield nominal nickel concentrations of two, eleven, and twenty weight percent relative to total composite mass, followed by overnight oven drying at one hundred ten degrees Celsius and calcination under flowing pure nitrogen at five hundred degrees Celsius for twelve hours to decompose acetate ligands.

Chemical quantification via inductively coupled plasma optical emission spectrometry following alkaline fusion digestion with lithium tetraborate confirmed that the synthesized solid catalysts achieved empirical nickel loadings extraordinarily close to nominal formulation values. Nitrogen physisorption measurements carried out at minus one hundred ninety-six degrees Celsius following prolonged high-vacuum thermal degassing revealed characteristic low-porosity type six adsorption isotherms consistent with graphitic carbonaceous nanostructures. Textural evaluations applying Brunauer-Emmett-Teller calculations and Barrett-Joyner-Halenda pore size distribution analyses established that nickel loadings up to eleven weight percent exerted negligible influence on support specific surface area or channel accessibility, whereas elevating the metallic content to twenty weight percent provoked clear reductions in both specific surface area and average pore diameter due to partial pore blockage by bulky metallic crystallites.

Powder X-ray diffraction patterns revealed distinctive graphitic diffraction reflections across all materials, dominated by the characteristic graphitic carbon reflection at twenty-five point seventy-five degrees two-theta, confirming that neither thermal pretreatment nor metal deposition disrupted the core structural lattice of the multiwall carbon nanotubes. Additional reflections corresponding to the face-centered cubic zero-valent metallic nickel phase at forty-four point twenty-five degrees two-theta emerged across all metallized samples, with peak intensity and definition scaling directly with overall metal loading. Crystallite size calculations executed via the Scherrer equation applied to diffraction profile line broadening yielded average nickel crystallite diameters of six point six nanometers for the two weight percent sample, nineteen nanometers for the eleven weight percent sample, and twenty-five nanometers for the twenty weight percent catalyst, while complementary Raman spectroscopy showed prominent D and G bands at thirteen forty-eight and fifteen eighty inverse centimeters with an intensity ratio of one point zero eighty-seven.

Microscopic morphological evaluations utilizing field-emission scanning electron microscopy and high-resolution transmission electron microscopy coupled with energy-dispersive X-ray spectrometry visually corroborated that increasing metal loading promoted significant particle agglomeration. For the two weight percent catalyst, transmission micrographs verified exceptionally uniform nanoparticle distribution across nanotube surfaces, exhibiting an average particle diameter of fourteen nanometers, a calculated metallic dispersion of seven point three percent, and a narrow size distribution concentrated between six and fifteen nanometers. Conversely, elevating the loading to eleven and twenty weight percent nickel generated broader, noticeably heterogeneous size distributions spanning overall ranges from three to thirty-three nanometers, where larger particles predominated on the external nanotube walls and decreased active metal surface exposure per unit mass.

Reducibility and surface functional group evolution were systematically investigated using temperature-programmed reduction and helium-flow temperature-programmed desorption connected to in-line quadrupole mass spectrometers. The reduction profiles tracking water generation showed distinct peaks between one hundred and six hundred degrees Celsius, indicating the presence of surface nickel oxide species undergoing reduction to metallic nickel, with maximum reduction rates occurring at two hundred eighty degrees Celsius for the two and twenty percent catalysts and shifting downward to two hundred degrees Celsius for the eleven percent sample. Simultaneous detection of methane above six hundred degrees Celsius marked the onset of hydrogen-mediated carbon gasification, identifying four hundred degrees Celsius as the optimal in situ pre-reduction ceiling to achieve complete nickel reduction while strictly avoiding mass loss from the carbonaceous support framework.

Catalytic evaluation experiments were conducted in a continuous-flow fixed-bed reactor operating under a total hydrogen pressure of one point forty-seven megapascals across reaction temperatures of two hundred seventy-five, three hundred, three hundred twenty-five, and three hundred fifty degrees Celsius. Two hundred milligrams of catalyst powder mixed with one-millimeter glass beads were pre-reduced in situ at five hundred degrees Celsius under pure hydrogen flow for four hours prior to continuous feeding of two volume percent guaiacol dissolved in analytical-grade heptane at fourteen point eight milliliters per minute alongside hundred milliliter per minute hydrogen co-feed. Reaction effluents analyzed through gas chromatography equipped with flame ionization detection demonstrated overall guaiacol conversion efficiencies ranging between fifteen and thirty-three percent, with conversions stabilizing between twenty-five and thirty percent across all three catalyst formulations at three hundred twenty-five degrees Celsius.

Despite achieving roughly comparable gross substrate conversion levels at three hundred twenty-five degrees Celsius, the catalysts exhibited dramatic disparities in their intrinsic turnover frequency, calculated as millimoles of guaiacol converted per second per accessible metallic surface site. The low-loaded two weight percent nickel catalyst achieved the highest turnover frequency across all operating temperatures, showing strong positive thermal sensitivity as turnover rates rose proportionally with heating. In striking contrast, the highly loaded twenty weight percent catalyst exhibited the lowest turnover frequency, which remained virtually stagnant across the entire temperature range because its bulky metallic agglomerates possessed a low proportion of accessible edge sites that operated near saturation capacity even under mild thermal activation.

Product selectivity profiles revealed that guaiacol transformation proceeded primarily through selective demethoxylation and aromatic ring hydrogenation rather than exhaustive deoxygenation. Across all operational conditions and metal loadings, cyclohexanol, phenol, and alkylated cresols constituted the overwhelming majority of detected products, whereas complete hydrodeoxygenation to non-oxygenated hydrocarbons like cyclohexane or benzene was negligible within the evaluated conversion window below thirty-five percent. Catalysts possessing small, highly dispersed nickel particles strongly favored aromatic ring saturation, producing cyclohexanol selectivity reaching up to seventy-five percent at three hundred degrees Celsius over the two weight percent formulation, whereas larger nickel particles in the twenty weight percent catalyst favored rapid desorption of unhydrogenated intermediates from planar terrace sites, leading to elevated yields of free phenol.

Extended four-hour continuous time-on-stream reaction trials demonstrated robust operational stability, displaying negligible decay in guaiacol conversion or product distribution at three hundred twenty-five degrees Celsius. Post-reaction thermogravimetric and differential thermal analyses performed on spent catalysts recovered after hydroprocessing confirmed remarkably low levels of carbonaceous coke deposition, displaying only minor mass loss peaks around three hundred ten degrees Celsius. High-temperature differential thermal oxidation peaks between five hundred fifteen and eight hundred twenty-five degrees Celsius reflected the eventual combustion of the underlying carbon nanotube walls, confirming that multiwall carbon nanotubes provide exceptional resistance against severe fouling while nickel particle dispersion serves as the primary structural determinant of reaction rate and product selectivity.

Subject of Research: Hydrodeoxygenation of bio-oil model compound guaiacol using nickel supported on multiwall carbon nanotubes

Article Title: The effect of Nickel nanoparticles supported on carbon nanotubes (MWCNT) and structural properties on product yields of the guaiacol hydrodeoxygenation

Article References: Caetano, T. J., Schmal, M., Hewer, T., de Oliveira, É. V., Dionizio, D. G. B., & Toniolo, F. S. (2026). The effect of Nickel nanoparticles supported on carbon nanotubes (MWCNT) and structural properties on product yields of the guaiacol hydrodeoxygenation. Brazilian Journal of Chemical Engineering. https://doi.org/10.1007/s43153-026-00690-4

Image Credits: AI Generated

DOI: 10.1007/s43153-026-00690-4

Keywords: hydrodeoxygenation, guaiacol, nickel nanoparticles, multiwall carbon nanotubes, turnover frequency, catalytic activity, metal dispersion, bio-oil upgrading, cyclohexanol, phenol, incipient wetness impregnation, temperature-programmed reduction, transmission electron microscopy, X-ray diffraction, thermogravimetric analysis, coke deposition, structure sensitivity

News Source: Bethany Barker. (November 26, 2026). Dispersed Nickel Nanoparticles on Carbon Nanotubes Triple Guaiacol Hydrodeoxygenation Rates. Scienmag.